LOCTITE ECI1006
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category
Main features
- Halogen free
- High conductivity
- Fine line screen printable
Product Description
LOCTITE ECI 1006 E&C is a halogen-free, conductive silver ink with a very high viscosity. Therefore it is suitable for fine line printing (50 µm line/spacing possible), offering good adhesion when being printed onto polyester foil and ITO.
LOCTITE ECI 1006 E&C is suitable for screen printing and is often used for printing circuits on flexible substrates to create touch screens, EL-lamps and solar cells.
Drying cycle
- 10 minutes @ 130°C
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
DIRECTIONS FOR USE
1. Surface Preparation
- No surface treatment is needed for ITO or etched ITO substrates.
2. Mixing/Dilution
- Mix thoroughly before use to ensure it is homogenous.
- Avoid rapid stirring, as this causes air entrapment.
- If needed, the ink can be diluted with up to 1 to 2% by weight maximum with DBE (dibasic ester). The solvent should be mixed in thoroughly, including scraping the sides of the container, for over a minute until it is homogenous and streak free.
3. Application
- LOCTITE ECI 1006 E&C is designed for fine line screen printing application.
- Recommended screen and printing parameters are:
Stainless Steel Screen, mesh 400
Emulsion Thickness , µm 10 to 12
Polyurethane Squeegee, durometer D90
Print Speed, in/sec 7 to 10
Snap-off Distance, mils 50 to 80