FREKOTE 700-NC
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- No Chlorinated Solvents
- High Gloss Finish
- No Contaminating Transfer
Product Description
LOCTITE® FREKOTE 700-NC™ is a solvent-based polymer mold release coating designed for composite and molded polymer manufacturing processes. This room-temperature-curing release agent delivers a clear, colorless coating that provides high gloss, high slip, and clean release characteristics without contaminating transfer or mold build-up. Suitable for mold temperatures from 13°C to 135°C, it is used with epoxy resins, polyester resins, thermoplastics, rubber compounds, and other molded polymers where consistent release performance is required. Its cured thermal stability of up to 400°C supports demanding molding environments and repetitive production cycles.
Key features
- High-performance mold release: Provides reliable release for epoxies, polyester resins, thermoplastics, rubber compounds, and most molded polymers.
- Clean, non-transfer coating: Delivers high gloss and high slip characteristics with no contaminating transfer or mold build-up.
- Wide operating temperature range: Applicable at mold temperatures from 13°C to 135°C with cured thermal stability up to 400°C.
Applications / Suitable for
- Composite molding operations
- Epoxy resin processing
- Polyester resin molding
- Thermoplastic molding
- Rubber molding applications
- Mold release coating programs requiring high-gloss finishes
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied properties and processing characteristics for LOCTITE® FREKOTE 700-NC™.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Clear, colorless | — | As supplied |
| Chemical Type | Solvent-based polymer | — | Product description |
| Specific Gravity | 0.755 - 0.764 | — | @ 25°C |
| Application Temperature | 13 - 135 | °C | Mold surface temperature |
| Cure Type | Room temperature cure | — | Typical processing condition |
After-processing / final-state properties
Published final-state performance characteristics available from supplied source data.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Cured Thermal Stability | ≤400 | °C | Published cured-state characteristic |