BOSTIK SPA145FR-A

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

BOSTIK SPA145FR-A

Main features

  • Flame-Retardant Web Lamination
  • Controlled Adhesive Usage
  • Aerospace Interior Laminate Bonding

Product Description

Bostik SPA145FR-A is a one-component flame-retardant web adhesive in roll format for aerospace laminate bonding. The thin web-like construction provides a dry adhesive layer that can be placed between substrates before heat activation, while the web format gives manufacturers controlled adhesive usage and avoids spray overspray. Its flame-retardant positioning is intended for aerospace interior laminate constructions where a flame-retardant web adhesive is specified. Applications center on interior laminate bonding, keeping the grade within its defined aerospace web-adhesive role rather than general-purpose assembly bonding.

Key features

  • Flame-Retardant Web Construction: Thin hot-melt web format combines flame-retardant positioning with dry adhesive handling.
  • Controlled Adhesive Usage: Web application controls adhesive placement and avoids overspray associated with spray application.
  • Aerospace Interior Lamination: The grade is used for aerospace interior laminate bonding where a flame-retardant web is specified.

Applications

Aerospace interior laminate bonding where a flame-retardant web adhesive is specified.

Product Family

BOSTIK SPA145FR-A

Loading pricing…

Technical Specifications

General Properties
Basis Weight
17–71 g/m2
Color
White to off-white
Width
Up to 188 cm
Thermal Properties
Shear Adhesion Failure Test - SAFT
140 °C